Lsep 5e-5[m] Length of Separator Lpos 7.5e-4[m] Length of positive electrode Kpos 10[S/m] Conductivity of positive electrode epsilonl0 0.73 Initial porosity of positive electrode epsilons0 1-epsilonl0 Initial active material solid fraction of positive electrode epsilonsep 0.87 Porosity of separator rpos0 25e-9[m] Particle radius in the positive electrode apos0 3*epsilons0/rpos0 Initial active specific surface area in positive electrode Rfilm 50[ohm*m^2] Film resistance across Li2O2 film cLi0 1000[mol/m^3] Initial concentration of Li+ in electrolyte SolO2 0.40 Solubility factor of oxygen in electrolyte cO2ext 9.46[mol/m^3] External oxygen concentration in air at 1atm cO20 SolO2*cO2ext Initial oxygen concentration in positive electrode cmaxLi2O2 0.09[mol/m^3] Solubility limit of Li2O2 dissolved in electrolyte DLi 2.11e-9[m^2/s] Diffusion coefficient of Li+ in electrolyte DO2 7e-10[m^2/s] Oxygen diffusion coefficient kappaLi 1.085[S/m] Conductivity of Li+ in electrolyte tplus 0.2594 Transference number of Li+ in electrolyte dlnfdlnc -1.03 Activity dependence ka 1.11e-15[m/s] Reaction rate coefficient anodic current kc 3.4e-17[m^7/s/mol^2] Reaction rate coefficient cathodic current i0refLi 9.65e-1[A/m^2] Reference exchange current density Li metal Eeq 2.96[V] Equilibrium potential for oxygen reduction reaction n 2 Number of transferred electrons rhoLi2O2 2140[kg/m^3] Density of Li2O2 MLi2O2 45.88e-3[kg/mol] Molecular weight of Li2O2 rhocarbon 2260[kg/m^3] Density of carbon T 300[K] Temperature i_app -0.05*a[mA/cm^2] Applied current density a 1 Used in parametric sweep