L_pos 65[um] "Thickness of positive electrode" L_neg 85[um] "Thickness of negative electrode" L_electrolyte 45[um] "Thickness of electrolyte region" epss_pos 0.44 "Solid phase volume fraction of positive electrode" epss_neg 0.42 "Solid phase volume fraction of negative electrode" rp 5e-7[m] "Particle size in negative and positive electrodes" sigmas_neg 100[S/m] "Electric conductivity of negative electrode" sigmas_pos 1.13[mS/cm] "Electric conductivity of positive electrode" sigmal 0.02[S/m] "Electrolyte conductivity" i0ref_neg 3.04e-2[A/m^2] "Reference exchange current density negative electrode" i0ref_pos 5.43e-2[A/m^2] "Reference exchange current density positive electrode" SOC_0 1 "Initial SOC" C_rate 1 "C-rate parameter"